A249 TP310HCb簡(jiǎn)介

牌號(hào) A249 TP310HCb
美國(guó)UNS S31041
對(duì)應(yīng)標(biāo)準(zhǔn) ASTM A249/A249M-2018
焊接奧氏體鋼鍋爐、過(guò)熱器、熱交換器和冷凝器管
Welded Austenitic Steel Boiler, Superheater, Heat-Exchanger, and Condenser Tubes
歸類(lèi) 奧氏體不銹鋼
A249 TP310HCb 化學(xué)元素成分含量(%)
成分 C Si Mn P S Cr Ni 更多
最小值 0.04 - - - - 24 19 Nb(Cb):10C~1.10
最大值 0.1 1 2 0.045 0.03 26 22
碳當(dāng)量計(jì)算
A249 TP310HCb 機(jī)械性能
熱處理或狀態(tài)
抗拉強(qiáng)度
σb
Mpa
屈服點(diǎn)
σs
Mpa
斷后伸長(zhǎng)率或延伸率
δ
%
硬度
HBW
Solutioning Temperature 1040℃ ≥515 ≥205 ≥35 HRB
≤90
注1:Quenched in water or rapidly cooled by other methods.
注2:A solution treating temperature above 1950 °F [1065 °C] may impair resistance to intergranular corrosion after subsequent exposure to sensitizing conditions in the indicated grades. When specified by the purchaser, a lower temperature stabilization or re- solution anneal shall be used subsequent to the higher-temperature solution anneal prescribed in this table (See Supplementary Requirement S4).