全球鋼材百科網(wǎng)
A249 TP317簡(jiǎn)介

牌號(hào) A249 TP317
美國(guó)UNS S31700
對(duì)應(yīng)標(biāo)準(zhǔn) ASTM A249/A249M-2018
焊接奧氏體鋼鍋爐、過(guò)熱器、熱交換器和冷凝器管
Welded Austenitic Steel Boiler, Superheater, Heat-Exchanger, and Condenser Tubes
歸類 奧氏體不銹鋼
A249 TP317 化學(xué)元素成分含量(%)
成分 C Si Mn P S Cr Ni Mo
最小值 - - - - - 18 11 3
最大值 0.08 1 2 0.045 0.03 20 15 4
碳當(dāng)量計(jì)算
A249 TP317 機(jī)械性能
熱處理或狀態(tài)
抗拉強(qiáng)度
σb
Mpa
屈服點(diǎn)
σs
Mpa
斷后伸長(zhǎng)率或延伸率
δ
%
硬度
HBW
Solutioning Temperature 1040℃ ≥515 ≥205 ≥35 HRB
≤90
注:Quenched in water or rapidly cooled by other methods, at a rate sufficient to prevent reprecipitation of chromium carbides, as demonstrated by the capability of passing Practices A262, Practice E. The manufacturer is not required to run the test unless it is specified on the purchase order (See Supplementary Requirement S6). Note that Practices A262 requires the test to be performed on sensitized specimens in the low carbon and stabilized types and on specimens representative of the as-shipped condition of the other types. In the case of low-carbon types containing 3 % or more molybdenum, the applicability of the sensitizing treatment prior to testing shall be a matter for negotiation between the seller and purchaser.
1 近似對(duì)照表 奧氏體不銹鋼
中國(guó) 中國(guó)臺(tái)灣 日本 韓國(guó) 美國(guó) 德國(guó) 英國(guó)
GB ISC CNS JIS KS ASTM UNS DIN EN/DIN W-Nr. BS EN/BS
06Cr19Ni13Mo3 S31708 317 SUS 317 STS 317 317 S31700 X5CrNiMo 17-13 1.4449 317S16
2 近似對(duì)照表 奧氏體型耐熱鋼
中國(guó) 中國(guó)臺(tái)灣 日本 韓國(guó) 美國(guó) 德國(guó) 英國(guó)
GB ISC CNS JIS KS ASTM UNS DIN EN/DIN W-Nr. BS EN/BS
06Cr19Ni13Mo3
(0Cr19Ni13Mo3)
S31708 317 SUS 317 STS 317 317 S31700 X5CrNiMo 17-13 1.4449 317S16
3 近似對(duì)照表 奧氏體不銹鋼
中國(guó) 日本 美國(guó) 國(guó)際標(biāo)準(zhǔn)組織 歐標(biāo)
ISC JIS UNS ISO 數(shù)字牌號(hào) 數(shù)字牌號(hào)
S31708 SUS317 S31700 X6CrNiMo19-13-4 4445-317-00-U (1.4445)